DIN 51053, ISO 3187

Determination of Creep or Refractoriness Under Load

One cylindrical specimen (50 mm diameter x 50 mm high) is tested per firing. The percent linear change is recorded continuously during the heat-up and creep period under load. The minimum size required is a half brick. Standard conditions are 0.2 N/mm2 (29 psi) load and 50 hour hold.

  PER TEST OF 1 PER TEST OF 1 PER TEST OF 1
TEMPERATURE (50 hr hold) (100 hr hold) (RUL only)
1400°C or Less $900 $1135 $480
1400°C to 1500°C $1030 $1270 $620
1500°C to 1600°C $1160 $1410 $715
1600°C to 1650°C $1350 $1590 $810
1650°C to 1700°C $1420 $1675 $850
Other Test Conditions Quote Quote Quote

DOWNLOAD REQUEST FORM »

View Products by Category:

 

Search
clear

FROM THE BLOG...

Hot Disk Instruments added to Orton's Instrument Line

Orton is pleased to announce its partnership with Hot Disk of Gothenburg, Sweden representing Hot...

Jessica Putnam-Phillips on ClayShare

Jessica explains how Pyrometric cones help the firing process.  Click here to Watch her on ClayShare...

Sue McLeod and Witness Cones

We ran across this recent post from Sue McLeod that explains why she uses Witness Cones in her firings. ...