Alcoa Modified Aluminum Cup Penetration

The comparative resistance of refractory brick, mortars, or monolithics can be determined using this cup test, with 7075 aluminum alloy at 1500°F for 72 hours. Two 9" bricks are required. Before and after metal analysis is available at an additional cost of $170 per analysis.

$810 per test of 1 specimen
$1070 per test of 2 specimens