Determination of Creep or Refractoriness Under Load

One cylindrical specimen (50 mm diameter x 50 mm high) is tested per firing. The percent linear change is recorded continuously during the heat-up and creep period under load. The minimum size required is a half brick. Standard conditions are 0.2 N/mm2 (29 psi) load and 50 hour hold.

  PER TEST OF 1 PER TEST OF 1 PER TEST OF 1
TEMPERATURE (50 hr hold) (100 hr hold) (RUL only)
1400°C or Less $840 $1070 $455
1400°C to 1500°C $965 $1190 $585
1500°C to 1600°C $1085 $1315 $670
1600°C to 1650°C $1230 $1460 $755
1650°C to 1700°C $1295 $1530 $795
Other Test Conditions Quote Quote Quote

DOWNLOAD REQUEST FORM »

View Products by Category:

 

Search
clear

FROM THE BLOG...

2019 Introduction to Refractories Short Course

Orton's 2019 "Introduction to Refractories" short course is coming up in August. This course is an intensive...

New Laboratory Training Course Announced

LABORATORY TRAINING - THERMAL PROPERTIES OF REFRACTORIES - March 19, 20 & 21, 2019 A Three Day Course...

Introducing a new two day course: Advanced Thermal Properties of Refractories

ADVANCED THERMAL PROPERTIES OF REFRACTORIES - October 29 & 30, 2018 A Two Day Course Sponsored by...